articles This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/bync/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
Copyright © KIChE. All rights reserved.

All issues

Pyrolysis of Polystyrene in a Batch-Type Stirred Vessel

Korean Journal of Chemical Engineering, March 1999, 16(2), 161-165(5), 10.1007/BF02706830
downloadDownload PDF

Abstract

Isothermal pyrolysis of PS was investigated in the relatively low temperature range of 370 to 400℃, using a stirred tank of batch-type with respect to the liquid phase ; the gas phase was operated in an open system. To maintain an isothermal condition, the stirring speed was 80rpm. At the initial stage of pyrolysis at each temperature, the first-order kinetic law was found to be operative. The activation energy was evaluated to be 224kJ/mol, a value close to the previously reported one. The main liquid products were single and double aromatic ring species : styrene, α-methylstyrene, toluene and 1,3-diphenylpropane, 1,3-diphenylbutene. The yield of styrene was much larger than any other product and amounted to ca. 70% by weight. The present reactor, operated in an open system with respect to the gas phase, tends to suppress the scission of volatile diphenyl radicals because of short residence times of these radicals.

References

Carniti P, Beltrame PL, Armade M, Gervasini A, Audisio G, Ind. Eng. Chem. Res., 30(7), 1624 (1991) 
Ghim YS, HWAHAK KONGHAK, 30(2), 133 (1992)
Guyot A, Polym. Degrad. Stabil., 15, 219 (1986) 
Marsh JA, Cha CY, Guffey FD, Chem. Eng. Commun., 129, 69 (1994)
Kaminsky W, Janning T, Ikemura T, J. Appl. Polym. Sci., 29, 2561 (1984) 
Kaminsky W, Chem. Macromol. Symp., 48-49, 381 (1991)
Kim S, Chun HD, Korean J. Chem. Eng., 12(4), 448 (1995)
Poller RC, J. Chem. Technol. Biotechnol., 30, 152 (1980)
Schroeder UKO, Ebert KH, Hamielec AW, Makromol. Chem., 185, 991 (1984) 
Scott DS, Czernik SR, Radlein D, "Fast Pyrolysis of Waste Plastics," IGT Meeting, Orland, Florida, January (1990)
Shin BS, Seul SD, Korean J. Chem. Eng., 11(2), 74 (1994)
Sinn H, Kiminsky W, Janning T, Angew. Chem.-Int. Edit., 15, 660 (1976) 

The Korean Institute of Chemical Engineers. F5, 119, Anam-ro, Seongbuk-gu, 233 Spring Street Seoul 02856, South Korea.
TEL. No. +82-2-458-3078FAX No. +82-507-804-0669E-mail : kiche@kiche.or.kr

Copyright (C) KICHE.all rights reserved.

- Korean Journal of Chemical Engineering 상단으로