- This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/bync/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
Copyright © KIChE. All rights reserved.
All issues
Characterization of metal (Ba, Al, Si, V, and W)-incorporated TiO2 and toluene photodecomposition in the presence of H2O
Department of Life Science, College of Natural Sciences, Hanyang University, Seoul 133-791, Korea 1Research Institute of Industrial Science & Technology (RIST), Pohang, Gyeongbuk 790-600, Korea 2Department of Chemistry, College of Science, Yeungnam University, Gyeongsan, Gyeongbuk 712-749, Korea
Korean Journal of Chemical Engineering, November 2007, 24(6), 965-974(10), 10.1007/s11814-007-0106-7
Download PDF
Abstract
This study focused on toluene photodecomposition in the presence of H2O over metal (Ba, Al, Si, V, and W)-incorporated TiO2. The nanometer-sized, metal-TiO2 photocatalyst samples, including Ba2+, Al3+, Si4+, V5+, and W6+ ions, were prepared by using the solvothermal method. The X-ray photoelectron spectroscopy (XPS) results showed that the Ti-OH peak, which indicates hydrophilicity, increased with increasing Al and Si ion components but decreased with increasing Ba, V, and W ion components. The contact angles were distributed over the range of 0-10° on almost all films (200-nm thick) after irradiation for 2 h, and in particular approached 0° on the Al-TiO2 and Si-TiO2 nanometer-sized films after just 30 min. The toluene (100 ppm) photodecomposition in the continuous system increased in the order of Al-TiO2>Si-TiO2>pure TiO2>W-TiO2>Ba-TiO2>V-TiO2, and the maximum toluene conversion rate achieved was 45% over Al-TiO2 film after 120 min. The toluene conversion remarkably increased; however, over all photocatalysts, with H2O addition during the toluene photo-decomposed reaction, and in particular, the conversion reached up to 90% after 120 min over Al-TiO2 and Si-TiO2 with increased hydrophilicity. After photoreaction for 24 h, minimal carbon was deposited on the photocatalyst under both reaction conditions, with and without H2O addition, although the deposited carbon amounts were smaller for the former. These results confirmed that the hydrophilicity of the photocatalyst had a greater effect on toluene decomposition, while the photocatalytic deactivation could be retarded by H2O supplementation during toluene decomposition.
References
Lim TH, Kim SD, Korean J. Chem. Eng., 19(6), 1072 (2002)
Valenzuela MA, Bosch P, Jimenez-Becerrill J, Quiroz Q, Paez AI, J. Photochem. Photobiol. A-Chem., 148, 177 (2002)
Bessekhouad Y, Chaoui N, Trzpit M, Ghazzal N, Robert D, Weber JV, J. Photochem. Photobiol. A-Chem., 183, 218 (2006)
Karunakaran C, Anilkumar P, J. Mol. Catal. A-Chem., 265(1-2), 153 (2007)
Yu JC, Yu J, Ho W, Zhao J, J. Photochem. Photobiol. A-Chem., 148, 331 (2002)
Lee BY, Park SH, Lee SC, Kang M, Park CH, Choung SJ, Korean J. Chem. Eng., 20(5), 812 (2003)
Xin J, Chen XM, J. Cryst. Growth, 270(3-4), 547 (2004)
Kang M, Lee MH, Appl. Catal. A: Gen., 284(1-2), 215 (2005)
Liu Q, Wu X, Wang B. Liu Q, Mater. Res. Bull., 37, 2255 (2002)
Guan K, Lu B, Yin Y, Surf. Coat. Technol., 173, 219 (2003)
Kang M, J. Mol. Catal. A-Chem., 197(1-2), 173 (2003)
Kang M, Choung SJ, Park JY, Catal. Today, 87(1-4), 87 (2003)
Kim SB, Hwang HT, Hong SC, Chemisophere, 48, 437 (2002)
Muggli DS, Backes MJ, J. Catal., 209(1), 105 (2002)
Kang M, Lee SY, Chung CH, Cho SM, Han GY, Kim BW, Yoon KJ, J. Photochem. Photobiol. A-Chem., 144, 185 (2001)
Gogebakan M, Uzun O, J. Mater. Process. Technol., 153-154, 829 (2004)
Choi HJ, Kim JS, Kang M, Bull. Korean Chem. Soc., 28, 581 (2007)
Lee YC, Hong YP, Lee HY, Kim H, Jung YJ, Ko KH, Jung HS, Hong KS, J. Colloid Interface Sci., 267(1), 127 (2003)
Valenzuela MA, Bosch P, Jimenez-Becerrill J, Quiroz Q, Paez AI, J. Photochem. Photobiol. A-Chem., 148, 177 (2002)
Bessekhouad Y, Chaoui N, Trzpit M, Ghazzal N, Robert D, Weber JV, J. Photochem. Photobiol. A-Chem., 183, 218 (2006)
Karunakaran C, Anilkumar P, J. Mol. Catal. A-Chem., 265(1-2), 153 (2007)
Yu JC, Yu J, Ho W, Zhao J, J. Photochem. Photobiol. A-Chem., 148, 331 (2002)
Lee BY, Park SH, Lee SC, Kang M, Park CH, Choung SJ, Korean J. Chem. Eng., 20(5), 812 (2003)
Xin J, Chen XM, J. Cryst. Growth, 270(3-4), 547 (2004)
Kang M, Lee MH, Appl. Catal. A: Gen., 284(1-2), 215 (2005)
Liu Q, Wu X, Wang B. Liu Q, Mater. Res. Bull., 37, 2255 (2002)
Guan K, Lu B, Yin Y, Surf. Coat. Technol., 173, 219 (2003)
Kang M, J. Mol. Catal. A-Chem., 197(1-2), 173 (2003)
Kang M, Choung SJ, Park JY, Catal. Today, 87(1-4), 87 (2003)
Kim SB, Hwang HT, Hong SC, Chemisophere, 48, 437 (2002)
Muggli DS, Backes MJ, J. Catal., 209(1), 105 (2002)
Kang M, Lee SY, Chung CH, Cho SM, Han GY, Kim BW, Yoon KJ, J. Photochem. Photobiol. A-Chem., 144, 185 (2001)
Gogebakan M, Uzun O, J. Mater. Process. Technol., 153-154, 829 (2004)
Choi HJ, Kim JS, Kang M, Bull. Korean Chem. Soc., 28, 581 (2007)
Lee YC, Hong YP, Lee HY, Kim H, Jung YJ, Ko KH, Jung HS, Hong KS, J. Colloid Interface Sci., 267(1), 127 (2003)