Articles & Issues
- Language
- English
- Conflict of Interest
- In relation to this article, we declare that there is no conflict of interest.
- Publication history
-
Received January 2, 2021
Accepted April 26, 2021
- This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/bync/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
Copyright © KIChE. All rights reserved.
All issues
Preparation and characteristics of wavy form microchannel reactors coated with H-ZSM-5 for the endothermic decomposition reaction of methylcyclohexane
Department of Biochemical and Chemical Engineering, Dongguk University, Seoul 04620, Korea 1Agency for Defense Development, Jochiwongil 462, Daejeon, Yuseong 34186, Korea
pjhoon@dongguk.edu
Korean Journal of Chemical Engineering, July 2021, 38(7), 1394-1402(9), 10.1007/s11814-021-0823-3
Download PDF
Abstract
Endothermic decomposition reaction of methylcyclohexane (MCH) was conducted to solve problems of hypersonic flight as cooling technology. A wavy form microchannel reactor (WMCR) coated with H-ZSM-5 was used to improve this reaction. WMCR coated with H-ZSM-5 was simply prepared by using binder coating method. Field emission scanning electron microscope (FE-SEM) and energy dispersive spectroscopy (EDS) analysis were used to examine the surface of WMCR coated with H-ZSM-5. Endothermic decomposition reaction of MCH was carried out in a flow reactor under supercritical conditions (823 K and 50 bar) during 30min. The liquid products produced by catalytic reaction were analyzed by gas chromatograph-mass selective detector (GC-MSD) at 10, 20 and 30 min, respectively. The results show that an increase in H-ZSM-5 coating amount on WMCR surface for catalytic reaction had a trade-off relationship; the increase of catalysts on WMCR had a positive effect on overall improvement of heat sink (from 416.59 kJ/mol to 611.06 kJ/mol) but simultaneously negative effect for catalytic life time because of increase in catalytic deactivation (from 5.9% to 30%).
References
Shin MC, Moon JI, Jung JH, Jeong BH, Park JH, React. Kinet. Mech. Catal., 126, 761 (2019)
Gascoin N, Gillard P, Dufour E, Toure Y, J. Thermophys. Heat Transf., 21, 86 (2007)
Wickham DT, Engel JR, Rooney S, Hitch BD, J. Propul. Power, 24, 55 (2008)
Guo Y, Lin R, J. Zhejiang Univ.-SCI A, 6, 632 (2005)
Kim J, Park SH, Chun BH, Jeong BH, Han JS, Kim SH, Catal. Today, 185(1), 47 (2012)
Lee TH, Jeong H, Jeong BH, Han JS, Gim MY, Kim DH, Kim SH, Lee KB, Appl. Surf. Sci., 511, 145398 (2020)
Nixon AC, Henderson HT, Ind. Eng. Chem. Prod. Res. Dev., 5, 87 (1966)
E XTF, Zhang Y, Zou JJ, Wang L, Zhang XE, Ind. Eng. Chem. Res., 53(31), 12312 (2014)
Sobel DR, Spadaccini LJ, J. Eng. Gas. Turbines Power, 119, 344 (1997)
Jiang R, Liu G, He X, Yang C, Wang L, Zhang X, Mi Z, J. Anal. Appl. Pyrolysis, 92, 292 (2011)
Lander H, Nixon AC, J. Aircr., 8, 200 (1971)
Wu H, Li G, Appl. Catal. A: Gen., 423-424, 108 (2012)
Song KH, Jeong SK, Jeong BH, Lee KY, Kim HJ, Catalysts, 10, 1149 (2020)
Zhao HL, Meng FX, Guo W, Zou JJ, Zhang XW, J. Fuel Chem. Technol., 36, 462 (2008)
Hou LY, Dong N, Sun DP, Fuel, 103, 1132 (2013)
Liu B, Zhu Q, Qin LX, Li XJ, Li XY, Tang SY, Wang JL, J. Propul. Power, 32, 801 (2016)
Vasu SS, Davidson DF, Hong Z, Hanson RK, Energy Fuels, 23(1), 175 (2009)
Narayanaswamy K, Pitsch H, Pepiot P, Combust. Flame, 162(4), 1193 (2015)
Meng FX, Liu GZ, Qu SD, Wang L, Mang XW, Mi ZT, Ind. Eng. Chem. Res., 49(19), 8977 (2010)
Song KH, Jeong SK, Park KT, Lee KY, Kim HJ, Fuel, 276, 118010 (2020)
Liu GZ, Guo JH, Meng FX, Zhang XW, Wang L, Chin. J. Chem. Eng., 22(8), 875 (2014)
Liu B, Lu S, Liu E, Hu X, Fan J, Korean J. Chem. Eng., 35(4), 867 (2018)
Huang H, Zhu H, Zhang Q, Li C, Korean J. Chem. Eng., 36(2), 210 (2019)
Xue NH, Nie L, Fang DM, Guo XF, Shen JY, Ding WP, Chen Y, Appl. Catal. A: Gen., 352(1-2), 87 (2009)
Luo J, Bhaskar BV, Yeh YH, Gorte RJ, Appl. Catal. A: Gen., 478, 228 (2014)
Blasco T, Corma A, Martinez-Triguero J, J. Catal., 237(2), 267 (2006)
Sun H, Shen BX, Liu JC, Sep. Purif. Technol., 64(1), 135 (2008)
Holland BT, Subramani V, Gangwal SK, Ind. Eng. Chem. Res., 46(13), 4486 (2007)
Jasra RV, Tyagi B, Badheka YM, Choudary VN, Bhat TSG, Ind. Eng. Chem. Res., 42(14), 3263 (2003)
Altin O, Eser S, Ind. Eng. Chem. Res., 40(2), 596 (2001)
Guo W, Zhang XW, Liu GZ, Wang J, Zhao J, Mi ZT, Ind. Eng. Chem. Res., 48(18), 8320 (2009)
Yang G, Zhang X, Liu S, Yeung KL, Wang J, J. Phys. Chem. Solids, 68, 26 (2007)
Truter LA, Makgwane PR, Zeelie B, Roberts S, Bohringer W, Fletcher JCQ, Chem. Eng. J., 257, 148 (2014)
Avila P, Montes M, Miro EE, Chem. Eng. J., 109(1-3), 11 (2005)
Yao X, Zhang Y, Du L, Liu J, Yao J, Renew. Sust. Energ. Rev., 47, 519 (2015)
Suryawanshi PL, Gumfekar SP, Bhanvase BA, Sonawane SH, Pimplapure MS, Chem. Eng. Sci., 189, 431 (2018)
Kolb G, Hessel V, Chem. Eng. J., 98(1-2), 1 (2004)
Gavriilidis A, Angeli P, Cao E, Yeong KK, Wan YSS, Chem. Eng. Res. Des., 80(1), 3 (2002)
Kim MK, Pak SH, Shin MC, Park CG, Magnone E, Park JH, Korean J. Chem. Eng., 36(7), 1201 (2019)
Zamaro JM, Ulla MA, Miro EE, Catal. Today, 107-108, 86 (2005)
Argyle MD, Batholomew CH, Catalysts, 5, 145 (2015)
Lee TH, Shin MC, Jeong BH, Park JH, Kim SH, Lee KB, Catal. Today, 358, 116 (2020)
Moulijn JA, van Diepen AE, Kapteijn F, Appl. Catal. A: Gen., 212(1-2), 3 (2001)
Gascoin N, Gillard P, Dufour E, Toure Y, J. Thermophys. Heat Transf., 21, 86 (2007)
Wickham DT, Engel JR, Rooney S, Hitch BD, J. Propul. Power, 24, 55 (2008)
Guo Y, Lin R, J. Zhejiang Univ.-SCI A, 6, 632 (2005)
Kim J, Park SH, Chun BH, Jeong BH, Han JS, Kim SH, Catal. Today, 185(1), 47 (2012)
Lee TH, Jeong H, Jeong BH, Han JS, Gim MY, Kim DH, Kim SH, Lee KB, Appl. Surf. Sci., 511, 145398 (2020)
Nixon AC, Henderson HT, Ind. Eng. Chem. Prod. Res. Dev., 5, 87 (1966)
E XTF, Zhang Y, Zou JJ, Wang L, Zhang XE, Ind. Eng. Chem. Res., 53(31), 12312 (2014)
Sobel DR, Spadaccini LJ, J. Eng. Gas. Turbines Power, 119, 344 (1997)
Jiang R, Liu G, He X, Yang C, Wang L, Zhang X, Mi Z, J. Anal. Appl. Pyrolysis, 92, 292 (2011)
Lander H, Nixon AC, J. Aircr., 8, 200 (1971)
Wu H, Li G, Appl. Catal. A: Gen., 423-424, 108 (2012)
Song KH, Jeong SK, Jeong BH, Lee KY, Kim HJ, Catalysts, 10, 1149 (2020)
Zhao HL, Meng FX, Guo W, Zou JJ, Zhang XW, J. Fuel Chem. Technol., 36, 462 (2008)
Hou LY, Dong N, Sun DP, Fuel, 103, 1132 (2013)
Liu B, Zhu Q, Qin LX, Li XJ, Li XY, Tang SY, Wang JL, J. Propul. Power, 32, 801 (2016)
Vasu SS, Davidson DF, Hong Z, Hanson RK, Energy Fuels, 23(1), 175 (2009)
Narayanaswamy K, Pitsch H, Pepiot P, Combust. Flame, 162(4), 1193 (2015)
Meng FX, Liu GZ, Qu SD, Wang L, Mang XW, Mi ZT, Ind. Eng. Chem. Res., 49(19), 8977 (2010)
Song KH, Jeong SK, Park KT, Lee KY, Kim HJ, Fuel, 276, 118010 (2020)
Liu GZ, Guo JH, Meng FX, Zhang XW, Wang L, Chin. J. Chem. Eng., 22(8), 875 (2014)
Liu B, Lu S, Liu E, Hu X, Fan J, Korean J. Chem. Eng., 35(4), 867 (2018)
Huang H, Zhu H, Zhang Q, Li C, Korean J. Chem. Eng., 36(2), 210 (2019)
Xue NH, Nie L, Fang DM, Guo XF, Shen JY, Ding WP, Chen Y, Appl. Catal. A: Gen., 352(1-2), 87 (2009)
Luo J, Bhaskar BV, Yeh YH, Gorte RJ, Appl. Catal. A: Gen., 478, 228 (2014)
Blasco T, Corma A, Martinez-Triguero J, J. Catal., 237(2), 267 (2006)
Sun H, Shen BX, Liu JC, Sep. Purif. Technol., 64(1), 135 (2008)
Holland BT, Subramani V, Gangwal SK, Ind. Eng. Chem. Res., 46(13), 4486 (2007)
Jasra RV, Tyagi B, Badheka YM, Choudary VN, Bhat TSG, Ind. Eng. Chem. Res., 42(14), 3263 (2003)
Altin O, Eser S, Ind. Eng. Chem. Res., 40(2), 596 (2001)
Guo W, Zhang XW, Liu GZ, Wang J, Zhao J, Mi ZT, Ind. Eng. Chem. Res., 48(18), 8320 (2009)
Yang G, Zhang X, Liu S, Yeung KL, Wang J, J. Phys. Chem. Solids, 68, 26 (2007)
Truter LA, Makgwane PR, Zeelie B, Roberts S, Bohringer W, Fletcher JCQ, Chem. Eng. J., 257, 148 (2014)
Avila P, Montes M, Miro EE, Chem. Eng. J., 109(1-3), 11 (2005)
Yao X, Zhang Y, Du L, Liu J, Yao J, Renew. Sust. Energ. Rev., 47, 519 (2015)
Suryawanshi PL, Gumfekar SP, Bhanvase BA, Sonawane SH, Pimplapure MS, Chem. Eng. Sci., 189, 431 (2018)
Kolb G, Hessel V, Chem. Eng. J., 98(1-2), 1 (2004)
Gavriilidis A, Angeli P, Cao E, Yeong KK, Wan YSS, Chem. Eng. Res. Des., 80(1), 3 (2002)
Kim MK, Pak SH, Shin MC, Park CG, Magnone E, Park JH, Korean J. Chem. Eng., 36(7), 1201 (2019)
Zamaro JM, Ulla MA, Miro EE, Catal. Today, 107-108, 86 (2005)
Argyle MD, Batholomew CH, Catalysts, 5, 145 (2015)
Lee TH, Shin MC, Jeong BH, Park JH, Kim SH, Lee KB, Catal. Today, 358, 116 (2020)
Moulijn JA, van Diepen AE, Kapteijn F, Appl. Catal. A: Gen., 212(1-2), 3 (2001)