articles This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/bync/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
Copyright © KIChE. All rights reserved.

All issues

활성탄소섬유를 이용한 추진제 저장수명 연장

Propellant Shelf-life Extension by Surface-modified Activated Carbon Fiber

국방기술품질원, 130-650 서울시 동대문구 회기로 39번지 1충남대학교 화학공학과, 305-764 대전시 유성구 궁동 220
Defence Agency for Technology and Quality, 39 Hoegi-ro, Dongdaemun-gu, Seoul 130-650, Korea 1Department of Chemical Engineering, Chungnam National University, 220 Gung-dong, Yuseong-gu, Daejeon 305-764, Korea
Korean Chemical Engineering Research, August 2011, 49(4), 443-448(6), NONE Epub 3 August 2011
downloadDownload PDF

Abstract

추진제는 저장 중 발생되는 질소산화물로 인해서 저장수명이 짧아진다. 추진제의 저장수명을 연장할 목적으로 활성 탄소섬유로 추진제에서 발생하는 질소산화물을 흡착하였다. 활성탄소섬유에 폐추진제를 첨착시키고 열처리하여 표면을 개질한 결과 비표면적이 약간 감소하였으나 피리딘(pyridine), 피리돈(pyridone) 및 피롤(pyrrol) 등의 질소기능기가 생기는 것을 확인하였다. NO에 대한 흡착시험을 통해서 표면개질한 활성탄소섬유의 흡착능이 개질 이전의 활성탄소 섬유에 비해 약 2배 증가하였다. 그리고 추진제에 대한 가속수명시험 결과 표면개질한 활성탄소섬유를 동봉하면 추진제의 저장수명이 약 25% 증가하였다.
The propellant has a short shelf-life because of nitrogen oxides that were released from nitrocellulose decomposition. As-received and surface-modified ACFs were applied to remove the nitrogen oxides with intend to extend the shelf-life of propellant. The specific surface area of modified ACFs was slightly decreased but nitrogen function groups such as pyridine, pyridone and pyrrol were created on the surface of ACFs. As a result, the NO removal capacity of the surface-modified ACF by propellant waste increased about twice than that of the as-received ACF. The shelf-life of propellant was extended about 1.25 times by accompanying surface-modified ACF.

References

Thrower P (Ed.), Chemistry and Physics of Carbon, vol. 25, Marcel Dekker, New York, N.Y. (1997)
Chae JS, Ko KR, Jung CH, Rhee BS, Ryu SK, HWAHAK KONGHAK, 31(1), 99 (1993)
Kim YO, Ko KR, Park YT, Ryu SK, HWAHAK KONGHAK, 30(3), 347 (1992)
Ryu SK, High Temp.-High Pressure., 22(4), 345 (1990)
Isao M, Yozo K, Masuaki S, Shizuo K, Tomohiro H, Yorimasa S, Carbon., 38(2), 227 (2000)
Park SJ, Shin JS, Shim JW, Ryu SK, J. Colloid Interface Sci., 275(1), 342 (2004)
Byeon JH, Yoon HS, Yoon KY, Ryu SK, Hwang JH, Surf. & Coat. Technol., 202(15), 3571 (2008)
Lee YS, Kim YH, Hong JS, Suh JK, Cho GJ, Catal. Today, 120(3-4), 420 (2007)
Muniz J, Marban G, Fuertes AB, Appl. Catal. B: Environ., 27(1), 27 (2000)
Shirahama N, Mochida I, Korai Y, Choi KH, Enjoji T, Shimohara T, Yasutake A, Appl. Catal. B: Environ., 52(3), 173 (2004)
Raymundo-Piero E, Cazorla-Amors D, Linares-Solano A, Carbon., 41(10), 1925 (2003)
Yu J, Wu Y, Wang S, Ma X, Carbohydrate Polymer., 70(1), 8 (2007)
Wang MJ, Chang YI, Poncin-Epilla F, Surf. Interface Analysis., 37(3), 348 (2005)
Folly P, Mader M, CHIMIA International J. Chem., 58, 374 (2004)
Army Technical Manual TM 9-1300-214(with Change No.4), Department of the Army, Headquarters, Washington, D.C. (1990)
Lindblom T, Reactions in the System Nitro-cellulose/ Diphenylamine with special reference to the formation of a stabilizing product bonded to nitrocellulose, ACTA universitatis upsaliensis, Uppsala, Sweden (2004)
Borcherding R, Waste Manage., 17(2), 135 (1997)
Yoon KS, Ryu SK, Korean J. Chem. Eng., 27(6), 1882 (2010)
Biniak S, Szymaski G, Siedlewski J, SwiatkOwski A, Carbon., 35(12), 1799 (1997)
Kutics K, Suzuki M, “Adsorption of Organics on Surface Modified Activated Carbon Fibers,” The 2’nd Korea-Japan Symposium on Separation Technology, June 1-2, Seoul, 395 (1990)
Ryu SK, Kim SY, Gallego N, Edie DD, Carbon., 37(10), 1619 (1999)
Moreno-Castilla C, Lopez-Ramon MV, Carrasco-Marin F, Carbon., 38(14), 1995 (2007)
Shen W, Wang H, Liu Y, Guo Q, Zhang Y, Colloids. Surf. A., 308, 20 (2007)

The Korean Institute of Chemical Engineers. F5, 119, Anam-ro, Seongbuk-gu, 233 Spring Street Seoul 02856, South Korea.
Phone No. +82-2-458-3078FAX No. +82-507-804-0669E-mail : kiche@kiche.or.kr

Copyright (C) KICHE.all rights reserved.

- Korean Chemical Engineering Research 상단으로